Inconel 660 / Alloy 660 (UNS S66286 / SUH660 / GH2132) – Superalloy nke dabeere na ígwè na-eme ka mmiri sie ike maka ọrụ okpomọkụ dị elu

Nkọwa Dị Mkpirikpi:

Inconel 660 (UNS S66286 / SUH660 / GH2132 /W.Nr. 1.4980) bụ ihe e ji ígwè mee nke na-eme ka mmiri sie ike nke ọma, nke nwere ike dị elu ma na-eguzogide oxidation ruo 704°C (1300°F). Womic Steel na-enye Inconel 660 n'ọtụtụ ụdị ngwaahịa gụnyere paịpụ na-enweghị ntụpọ, paịpụ a na-agbakọta, ogwe ígwè, efere ígwè, eriri ígwè, eriri, flanges, ihe ndị e ji etinye ihe, forgings, waya, na ihe njide maka ngwa ụgbọelu, turbine gas, ụgbọ ala, nuklia, na petrochemical.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Kedu ihe bụ Inconel 660?

Inconel 660 bụ ihe eji ígwè emepụta nickel-chromium nke na-eme ka ọ sie ike site na mmiri ozuzo nke usoro γ' [Ni₃(Al,Ti)] n'oge ọgwụgwọ okpomọkụ na-aka nká. Ihe a na-emepụta nwere ihe dị ka 24-27% nickel, 13.5-16% chromium, yana mgbakwunye nke titanium (1.9-2.35%), aluminom (0.10-0.35%), molybdenum (1.0-1.5%), na vanadium (0.10-0.50%). Emebere ya maka ngwa ndị chọrọ ike dị elu ruo 700°C yana ezigbo iguzogide oxidation na corrosion.

A maara ọkwa 660 maka:

●Ike okpomọkụ dị eluruo 704°C (1300°F)

●Ezigbo iguzogide mgbawana okpomọkụ dị elu

●Mmiri siri ikesite na ọgwụgwọ okpomọkụ ịka nká nkịtị

●Nguzogide oxidation dị mmaruo 815°C

●Nguzogide izu ike nrụgidena okpomọkụ dị elu

●Na-abụghị magnetikihe onwunwe

●Ịrụpụta ihe nke ọmana ike igwe

Ngwakọta Kemịkalụ

Ihe UNS S66286 (ASTM) SUH660 (JIS) GH2132 (GB) Ọrụ
Nickel (Ni) 24.0 – 27.0 24.0 – 27.0 24.0 – 27.0 Austenite stabilizer, iguzogide nchara
Chromium (Cr) 13.5 – 16.0 13.5 – 16.0 13.5 – 16.0 Nguzogide oxidation, carbide mbụ
Molybdenum (Mo) 1.0 – 1.5 1.0 – 1.5 1.0 – 1.5 Ime ka ngwọta siri ike sikwuo ike
Titanium (Ti) 1.90 – 2.35 1.90 – 2.35 1.90 – 2.35 Mmiri ozuzo γ, ike ọgwụgwụ afọ
Aluminom (Al) 0.10 – 0.35 ≤ 0.35 ≤ 0.35 Mmiri ozuzo γ
Vanadium (V) 0.10 – 0.50 0.10 – 0.50 0.10 – 0.50 Nkacha mma ọka, carbide mbụ
Borọn (B) 0.003 – 0.010 0.001 – 0.010 0.001 – 0.010 Ime ka ókèala ọka sie ike
Kobalt (Co) ≤ 1.00 ≤ 1.00 ≤ 1.00 Ihe fọdụrụ
Ígwè (Fe) Nhazi nguzozi Nhazi nguzozi Nhazi nguzozi Ihe bụ isi
Kabọn (C) ≤ 0.08 ≤ 0.08 ≤ 0.08 Carbide mbụ
Silikọn (Si) ≤ 1.00 ≤ 1.00 ≤ 1.00 Ihe na-eme ka ọ ghara ịdị ọcha
Manganese (Mn) ≤ 2.00 ≤ 2.00 ≤ 2.00 Ihe na-eme ka ọ ghara ịdị ọcha
Fọshọrọs (P) ≤ 0.025 ≤ 0.040 ≤ 0.030 adịghị ọcha
Sọlfọ (S) ≤ 0.025 ≤ 0.030 ≤ 0.020 adịghị ọcha

Njirimara Mekaniki

Ọnọdụ Annealed (Agwọchara Ngwọta)

Akụ na ụba ASTM A453 ọkwa 660 Uru
Ike ọdụdọ ≤ 724 MPa (105 ksi)  
Ike Mmepụta (Mbelata 0.2%) –  
Ogologo ≥ 25%  
Ike siri ike ≤ 91 HRB

Ọnọdụ Ndị Agadi (Mmiri ozuzo siri ike)

Akụ na ụba ASTM A453 ọkwa 660 A Na-enweta Nkịtị
Ike ọdụdọ ≥ 965 MPa (140 ksi) 1,000 – 1,100 MPa
Ike Mmepụta (Mbelata 0.2%) ≥ 655 MPa (95 ksi) 700 – 800 MPa
Ogologo ≥ 15% 18 – 25%
Ike siri ike 24 – 35 HRC 28 – 32 HRC
Ike Ịrịgharị (650°C, 100h) ≈ 240 MPa  
Ike Ịrịgharị (700°C, 100h) ≈ 210 MPa

Njirimara Anụ Ahụ

Akụ na ụba Uru
Njupụta 7.95 g/cm³
Oke agbaze 1371 – 1427°C
Ọgbakọ okpomọkụ 15.0 W/m·K na 150°C
Ọnụọgụ nke Mgbasawanye Okpomọkụ 16.8 × 10⁻⁶/°C (20-100°C)
Modulu Elastic 201 GPA
Ịgafe magnetik Na-abụghị magnetik

Uru dị mkpa nke Inconel 660

Ike Okpomọkụ Dị Elu– Inconel 660 na-ejigide ike nrụgide dị elu, ike ọgwụgwụ, na ike mgbawa ruo 704°C. Usoro γ' nke na-eme ka mmiri ozuzo sie ike na-enye ike okpomọkụ dị elu karịa ígwè austenitic anaghị agba nchara nkịtị. A na-ejikarị alloy ahụ eme ihe maka bolt na ihe njide turbine ebe iguzogide ntụrụndụ dị oke mkpa.

Ezigbo Mgbochi Mmebi-Mgbawa– Alloy ahụ na-egosipụta ike dị egwu n'ikuku na okpomọkụ dị elu. Ndụ ịrị elu na 650°C gafere awa 1,000 n'okpuru nrụgide dị ala, na-eme ka ọ bụrụ ihe a pụrụ ịtụkwasị obi maka ọrụ ogologo oge dị elu na okpomọkụ.

Ezi Oxidation na Nguzogide Nrụgide– Site na ọdịnaya chromium nke 13.5-16%, Inconel 660 na-enye ezigbo iguzogide oxidation, scaling, na corrosion dị elu. Alloy ahụ na-arụ ọrụ nke ọma na gburugburu ebe oxidation ruo 815°C ma na-eguzogide ọtụtụ ihe mgbochi corrosion.

Mmiri siri ike– Mmiri nwere ike ime ka Inconel 660 sie ike site na ọgwụgwọ okpomọkụ nke na-aka nká. Usoro ịka nká nkịtị (675-705°C, awa 12-16) na-emepụta ihe ndị dị mma maka igwe ma na-enye ezigbo nguzogide nkwụsịtụ nrụgide, nke dị oke mkpa maka itinye bolting.

Nguzogide Ike ọgwụgwụ nke Ọma– Alloy ahụ na-enye ezigbo iguzogide ike ọgwụgwụ na ike ọgwụgwụ okpomọkụ, na-eme ka ọ dabara adaba maka ihe ndị a na-ebu ibu n'oge okpomọkụ dị elu. Nke a dị mkpa karịsịa maka ngwa turbine na ihe ndị dị na injin.

Ezigbo nrụzi na arụmọrụ ọrụ– Inconel 660 nwere ike ịrụ ọrụ nke ọma karịa ọtụtụ ihe ndị ọzọ dị oke mma. Enwere ike ịkpụ ya ngwa ngwa, rụọ ọrụ ọkụ, ma jiri ya mee ihe n'oyi. A na-eji TIG, MIG, na njikọta ike agbado ya site na iji ígwè ndị kwesịrị ekwesị.

Uru dị mkpa nke Inconel 660

Ike Okpomọkụ Dị Elu– Inconel 660 na-ejigide ike nrụgide dị elu, ike ọgwụgwụ, na ike mgbawa ruo 704°C. Usoro γ' nke na-eme ka mmiri ozuzo sie ike na-enye ike okpomọkụ dị elu karịa ígwè austenitic anaghị agba nchara nkịtị. A na-ejikarị alloy ahụ eme ihe maka bolt na ihe njide turbine ebe iguzogide ntụrụndụ dị oke mkpa.

Ezigbo Mgbochi Mmebi-Mgbawa– Alloy ahụ na-egosipụta ike dị egwu n'ikuku na okpomọkụ dị elu. Ndụ ịrị elu na 650°C gafere awa 1,000 n'okpuru nrụgide dị ala, na-eme ka ọ bụrụ ihe a pụrụ ịtụkwasị obi maka ọrụ ogologo oge dị elu na okpomọkụ.

Ezi Oxidation na Nguzogide Nrụgide– Site na ọdịnaya chromium nke 13.5-16%, Inconel 660 na-enye ezigbo iguzogide oxidation, scaling, na corrosion dị elu. Alloy ahụ na-arụ ọrụ nke ọma na gburugburu ebe oxidation ruo 815°C ma na-eguzogide ọtụtụ ihe mgbochi corrosion.

Mmiri siri ike– Mmiri nwere ike ime ka Inconel 660 sie ike site na ọgwụgwọ okpomọkụ nke na-aka nká. Usoro ịka nká nkịtị (675-705°C, awa 12-16) na-emepụta ihe ndị dị mma maka igwe ma na-enye ezigbo nguzogide nkwụsịtụ nrụgide, nke dị oke mkpa maka itinye bolting.

Nguzogide Ike ọgwụgwụ nke Ọma– Alloy ahụ na-enye ezigbo iguzogide ike ọgwụgwụ na ike ọgwụgwụ okpomọkụ, na-eme ka ọ dabara adaba maka ihe ndị a na-ebu ibu n'oge okpomọkụ dị elu. Nke a dị mkpa karịsịa maka ngwa turbine na ihe ndị dị na injin.

Ezigbo nrụzi na arụmọrụ ọrụ– Inconel 660 nwere ike ịrụ ọrụ nke ọma karịa ọtụtụ ihe ndị ọzọ dị oke mma. Enwere ike ịkpụ ya ngwa ngwa, rụọ ọrụ ọkụ, ma jiri ya mee ihe n'oyi. A na-eji TIG, MIG, na njikọta ike agbado ya site na iji ígwè ndị kwesịrị ekwesị.

Ọgwụgwọ Okpomọkụ nke Inconel 660

Inconel 660 bụ ihe na-eme ka mmiri sie ike nke chọrọ ọgwụgwọ okpomọkụ kpọmkwem iji nweta ihe onwunwe kachasị mma:

Mbelata Ngwọta (Ọnọdụ A):

●Okpomọkụ:980 – 1010°C (1800 – 1850°F)

●Oge Mmịpụta:1 awa

●Ịjụ oyi:Oyi ngwa ngwa (mmanụ ma ọ bụ mmiri na-agbanyụ)

●Ebumnuche:Gbazee ihe niile na-ebute mmiri, nweta otu usoro austenite

●Nsonaazụ:Ọnọdụ dị nro, dị irè, dị njikere maka ịkpụ na igwe

Mmebi Mmiri Na-esi Ike (Ịka Nka – Ọnọdụ B):

●Okpomọkụ:675 – 705°C (1250 – 1300°F)

●Oge Mmịpụta:Awa 12 – 16

●Ịjụ oyi:Ikuku oyi

●Ebumnuche:Ụdị Ni₃(Al,Ti) γ' na-ebuli elu maka ike

●Nsonaazụ:Ike kachasị elu na nguzogide na-asọ asọ

Ịka nká ugboro abụọ (Nhọrọ):

● Ogbo Mbụ: 705°C ruo awa iri na isii, ọkụ ahụ jụrụ oyi ruo 620°C

● Nkeji nke Abụọ: 620°C ruo awa iri na isii, ikuku jụrụ oyi

●Ebumnuche:Mee ka iguzogide nchekasị dịkwuo mma maka ngwa bolting

Ụdị Ngwaahịa dị site na Womic Steel

Paịpụ Na-enweghị Ntụpọ na Tube Na-enweghị Ntụpọ

●Dayameta Mpụta:6mm – 200mm

●Ọkpụrụkpụ Mgbidi:1mm – 25mm

●Ogologo:Ruo mita iri na abụọ

●Ụkpụrụ:ASTM B639, ASTM B983, AMS 5731, AMS 5732, AMS 5737, AMS 5895

●Ngwa:Paịpụ usoro okpomọkụ dị elu, ọkpọkọ mgbanwe okpomọkụ, ahịrị ngwaọrụ, ọkpọkọ ikuku

●Isi okwu:Paịpụ Inconel 660 enweghị ntụpọ, tube Grade 660, paịpụ UNS S66286, tube SUH660, paịpụ 1.4980 enweghị ntụpọ

Ogwe ígwè (Gburugburu, Akụkụ anọ, Dị larịị, Hex)

●Dayameta:6mm – 300mm

●Elu:A na-akpọgharị ọkụ, na-egbuke egbuke (oyi na-atụ), Ala, Atụgharịrị

●Ụkpụrụ:ASTM A453, ASTM B639, AMS 5731, AMS 5732, AMS 5734, AMS 5737

●Ngwa:Bọltị turbine, ihe njide, studs, shafts, ogwe valvụ, ngwaahịa igwe

●Isi okwu:Ogwe gburugburu Inconel 660, Ogwe ọkwa 660, mkpanaka SUH660, ASTM A453 Akara 660, ihe njide okpomọkụ dị elu

Efere ígwè na mpempe akwụkwọ

●Ọkpụrụkpụ:1mm – 100mm

●Obosara:Ruo 2000mm

●Ụkpụrụ:AMS 5525, AMS 5858

●Ngwa:Akụkụ arịa nrụgide, akụkụ nhazi, oghere flange

●Isi okwu:Efere Inconel 660, mpempe akwụkwọ Grade 660, efere alloy, efere okpomọkụ dị elu

Ígwè na eriri ígwè

●Ọkpụrụkpụ:0.5mm – 4.0mm

●Obosara:10mm – 1000mm

●Ụkpụrụ:AMS 5525

●Ngwa:Ihe ndị e kere eke, bellows, stampings

●Isi okwu:Inconel 660 eriri, eriri, eriri okpomọkụ dị elu

Flanges na ihe ndị dị na ya

●Ụdị:Olu ịgbado ọkụ, slip-On, blind, socket weld, eri.

●Nha:1/2" – 24"

●Ọkwa Nrụgide:Klas nke 150 – Klas nke 2500

●Ụkpụrụ:ASTM A453, ASME B16.5

●Isi okwu:Flanges Inconel 660, ihe ndị dị na ọkwa 660

Ngwakọta

●Ụdị:Mgbaaka, diski, ogwe, ahụ valvụ, geometri omenala

●Ibu:Ruo 3,000kg kwa ibe

●Ụkpụrụ:ASTM A453, AMS 5731

●Isi okwu:Inconel 660 na-akpụ akpụ, mgbanaka e ji ígwè rụọ, ihe e ji ígwè rụọ

Ihe njide (bolts, akụ, studs)

●Ụdị:Bọltị Hex, skru isi okpu socket, boltị Stud, mkpanaka e ji eriri mee, mkpụrụ, ihe nhicha

●Nha:M2 – M100, 1/4" – 4"

●Ụkpụrụ:ASTM A453 Ọkwa 660, ASTM B637

●Ngwa:Bọltị turbine, njikọ flange okpomọkụ dị elu, ihe njikọ nhazi

●Isi okwu:Bọltị Inconel 660, Bọltị stud nke ọkwa 660, ihe njide okpomọkụ dị elu, blọtị turbine

Valvụ 660 nke ọkwa

●Ụdị:Valvụ bọọlụ, valvụ ọnụ ụzọ ámá, valvụ ụwa, valvụ nlele

●Nha:1/2" – 12"

●Ọkwa Nrụgide:Klas nke 150 – Klas nke 2500

●Oke okpomọkụ:-196°C ruo +704°C

●Ụkpụrụ Nhazi:API 608, API 6D, ASME B16.34

●Mmegharị:Ntuziaka, Pneumatic, Elektrọnik

●Ngwa:Mwepụ usoro okpomọkụ dị elu, ahịrị uzuoku turbine, njikwa turbine gas

Klas 660 megide Inconel 718: Ntụnyere

Inconel 660 na Inconel 718 bụ ihe ndị na-eme ka mmiri sie ike, mana ha nwere ọdịiche dị iche:

Inconel 660 - Alloy okpomọkụ dị elu nke dabere na ígwè

●Ihe Dị Mkpa:Ígwè (nhazi) nwere 24-27% Ni

●Usoro ime ka ike sie ike:γ' (Ni₃(Al,Ti))

●Ike nrụgide (agadi):≥ 965 MPa

●Ike okpomọkụ:Ruo 704°C

●Ngwa ndị dị mkpa:Bọltịn turbine, ihe njide, studs, ihe ndị mejupụtara injin jet

●Ọnụ ego:Ọ dị ọnụ ala karịa 718 nke dabere na nickel

●Inconel 718 - Superalloy nke dabere na Nickel

●Ihe Dị Mkpa:Nickel (50-55%) na 18-20% Fe

●Usoro ime ka ike sie ike:γ' (Ni₃Al) + γ'' (Ni₃Nb)

●Ike nrụgide (agadi):≥ 1,240 MPa

●Ike okpomọkụ:Ruo 700°C

●Ngwa ndị dị mkpa:Diski turbine, moto rọketi, mmanụ na gas HPHT

Mgbe ị ga-ahọrọ ọkwa 660:Ngwa ndị chọrọ bolting na njikọ dị elu, ihe ndị dị na injin jet, bolts turbine, na ụgbọala nwere arụmọrụ dị elu ebe ọnụ ahịa bụ ihe dị mkpa na ike dị elu ruo 700°C dị mkpa.

Mgbe ị ga-ahọrọ Inconel 718:Ngwa ndị chọrọ oke ike okpomọkụ dị elu, ike mgbawa, na iguzogide ihe na-asọ asọ na okpomọkụ ruo 700°C ebe ọnụ ahịa adịghị oke mkpa.

Ụkpụrụ na Nkọwapụta

Ọkọlọtọ Nkọwa
Nhọpụta UNS S66286
Nọmba Ọrụ 1.4980
AISI/SAE 660
ASTM A453 Nkọwapụta ọkọlọtọ maka bolting okpomọkụ dị elu
ASTM B639 Ogwe/mkpanaka alloy dị elu
AMS 5525 Efere/mpempe akwụkwọ/ebe a na-adọba
AMS 5731 Ogwe, waya, ihe mkpuchi
AMS 5732 Ogwe, waya, ihe mkpuchi
AMS 5734 Ogwe, waya, ihe mkpuchi
AMS 5737 Pipe na tube
AMS 5895 Ogwe, waya, ihe mkpuchi
JIS SUH660
GB/T GH2132
ndị Yuropu 1.4980 / X6NiCrTiMoV25-15-2
ISO X6NiCrTiMoV25-15-2

Ngwa nke Inconel 660

ụgbọelu– A na-eji Inconel 660 eme ihe nke ukwuu na injin jet na gas turbine gụnyere turbine bolts, compressor disks, turbine casings, afterburner parts, thrust reversers, na engine loading hardware. Nchikota ya nke ike okpomọkụ dị elu, ike ọgwụgwụ, na iguzogide oxidation na-eme ka ọ dị mma maka ngwa ikuku dị mkpa. Alloy ahụ bụ ihe a na-ejikarị eme ihe maka bolts injin jet na ihe njide na-arụ ọrụ na okpomọkụ ruo 700°C.

Mmepụta Ike Turbine Gas– A na-eji alloy a eme ihe maka bolts turbine, studs, na ihe njikọ na turbines gas ụlọ ọrụ mmepụta ihe, turbines uzuoku, na ụlọ ọrụ ike okirikiri jikọtara ọnụ. Nguzogide ya megide nkwụsịtụ nrụgide na okpomọkụ dị elu na-eme ka njikọ bolts a pụrụ ịdabere na ya ruo ogologo oge ọrụ.

Ụgbọala– A na-eji Inconel 660 eme ihe n'ụlọ turbocharger, ihe ndị na-emepụta ihe na-ekpo ọkụ, ihe ndị dị na injin dizel, na ihe ndị na-ejikọ ụgbọala dị elu. Ike ya iguzogide okpomọkụ gas na-ekpo ọkụ na ịgbagharị okpomọkụ na-eme ka ọ dabara adaba maka injin ọgbara ọhụrụ nwere arụmọrụ dị elu na nke nwere turbocharged.

Ike nuklia– A na-eji alloy ahụ eme ihe na ihe ndị mejupụtara ihe na-eme ka ihe dị n'ime nuklia, ihe ndị dị n'ime ya, usoro njikwa mkpanaka, na ihe ndị na-ejide okpomọkụ dị elu nke chọrọ ntụkwasị obi ogologo oge na iguzogide radieshon neutron.

Nhazi Petrochemical– A na-eji Inconel 660 eme ihe na reactor kemịkalụ dị elu, tubes ndị na-eme mgbanwe, ihe ndị dị na ọkụ, na ọkpọkọ usoro nke chọrọ ike na iguzogide oxidation na okpomọkụ dị elu.

Ịgbado Okpomọkụ Dị Elu– Ọkwa 660 bụ ihe a na-ejikarị eme ihe maka itinye bolting n'okpomọkụ dị elu. A na-akọwapụta bolts na studs ASTM A453 Ọkwa 660 nke ọma maka flanges arịa nrụgide, casings turbine, na njikọ paịpụ dị elu nke chọrọ iguzogide creep na stress relief.

Ajụjụ Ndị A Na-ajụkarị

Ajụjụ: Gịnị bụ Inconel 660?

A: Inconel 660 (UNS S66286 / SUH660 / GH2132) bụ ihe na-eme ka mmiri ozuzo sie ike nke e ji ígwè mee, nke nwere ike dị elu ruo 704°C. Mmiri ozuzo γ na-eme ka ọ sie ike site na ọgwụgwọ okpomọkụ nke mere ka ọ dị nká, a na-ejikwa ya eme ihe nke ọma maka bolt turbine, ihe njide, na ihe ndị dị na injin jet.

Ajụjụ: Kedu ihe dị iche n'etiti ọkwa 660 na Inconel 718?

A: E ji ígwè mee Inconel 660 (nwere 24-27% Ni, Fe nguzozi) yana ike nrụgide ≥ 965 MPa, ebe Inconel 718 dabere na nickel (50-55% Ni) yana ike nrụgide ≥ 1,240 MPa. Ọkwa 660 dị ọnụ ala karịa ma jiri ya mee ihe nke ukwuu maka ịgbado ọkụ; a na-eji Inconel 718 eme ihe maka ike kachasị elu.

Q: Kedu okpomọkụ ọrụ kachasị elu maka Inconel 660?

A: A na-enye Inconel 660 ọkwa maka ọrụ na-aga n'ihu ruo 704°C (1300°F). Maka iguzogide oxidation, njem obere oge ruo 815°C (1500°F) ga-ekwe omume. Ike nke na-agagharị agagharị na-ebelata nke ukwuu karịa 700°C.

Q: Inconel 660 ọ dị mfe ịgbado ọkụ?

A: Ee, enwere ike iji usoro ịgbado ọkụ TIG, MIG, na iguzogide Inconel 660 gbado ọkụ. Agbanyeghị, ịgbado ọkụ chọrọ njikwa nke ọma nke ntinye okpomọkụ na nhọrọ ígwè iji zere mgbawa ọkụ. A na-achọ ịgbado ọkụ na ịka nká nke ngwọta mgbe ịgbado ọkụ gasịrị iji weghachi ihe onwunwe igwe.

Ajụjụ: Kedu ihe Inconel 660 pụtara na ndị China?

A: Ihe nha Inconel 660 nke ndị China bụ GH2132 (高温合金) maka ojiji ikuku na okpomọkụ dị elu, ihe nhata nke ndị Japan bụ SUH660.

Q: Kedu ụdị ngwaahịa dị maka Inconel 660?

A: Womic Steel na-enye Inconel 660 na paịpụ na-enweghị ntụpọ, paịpụ a gbanyere agbaze, ogwe ígwè, efere ígwè, eriri ígwè, eriri, flanges, ihe ndozi, forgings, waya, ihe njide, na valvụ. Nkọwapụta ngwaahịa zuru oke na oke nha dị na ngalaba nnweta ngwaahịa.

Q: Inconel 660 ọ chọrọ ọgwụgwọ okpomọkụ?

A: Ee. Inconel 660 chọrọ ka a na-eme ka mmiri ghara ịdị ọcha (980-1010°C) wee mee ka ọ dị ọcha (675-705°C ruo awa 12-16) iji nweta ihe ndị kacha mma maka igwe. Ọgwụgwọ ịka nká na-akpali usoro γ maka ime ka ọ sie ike.

Kpọtụrụ Womic Steel

Weebụsaịtị: www.womicsteel.com
Ozi ịntanetị: sales@womicsteel.com

Ekwentị / WhatsApp / WeChat:

Victor: +86 15575100681

Jack: +86 18390957568

Womic Steel – Onye mmekọ gị a pụrụ ịtụkwasị obi maka Inconel 660 / Grade 660 (UNS S66286, SUH660, GH2132) paịpụ na-enweghị ntụpọ, ogwe ígwè, efere ígwè, eriri ígwè, flanges, ihe ndị e ji etinye ihe, ihe ndị e ji achọ mma, na ihe e ji ejikọ ihe maka ikuku, turbine gas, mmepụta ike, na ngwa bolting okpomọkụ dị elu n'ụwa niile. Enwere ike ịchọta ihe niile, asambodo otu nhazi, na akwụkwọ EN 10204 Ụdị 3.1/3.2.